What is tempering of elastomers?

Tempering is a controlled heat treatment in which a material is heated to a temperature below its melting point for a specified period of time to adjust the molecular structure and reduce internal stresses. In elastomer components, tempering is used in some rubber compounds to ensure complete crosslinking, to allow volatile components in the component to diffuse, or to adjust the morphology.

1. What happens during the tempering of elastomers?

Some Rubber compounds They must be tempered after vulcanization. Whether a component needs to be tempered depends on the chemical composition of the compound. These components already have the final shape, but require an additional tempering process to achieve the desired component properties.

Refilting
The network of the rubber is after the Vulcanisation In the tool, the thick-walled component areas do not necessarily reach the required reaction temperature later than the thin areas due to limited heat conduction. After demolding, reactive groups, crosslinkers, or crosslink fragment may still be present. During tempering, a higher crosslink density also influences hardness, modulus of elasticity, tensile elongation, and residual compressive deformation. The direction and magnitude of the change depend on the Polymer, fillers, cross-linking agents, Additives and the state of interconnectedness achieved in the tool already.

Migration of fugitive components
During heating in the oven, volatile substances from the interior of the component diffuse to the surface and are transported away by the ambient air. These include decomposition products of crosslinkers, moisture, low-molecular-weight polymer components, and components of processing aids. Thick-walled molded parts require more time than thin seals, because the volatile components must travel longer distances before diffusing. As particles from the component migrate, mass, dimensions, and the odor of the component may also change slightly during heating.

Reducing internal tensions
During vulcanization in the mold, temperature differences and internal stresses are created. Tempering increases the flexibility of the polymer chains, allowing some of the stresses to dissipate. Form-weak or thin-walled parts must be adequately supported during the treatment, as otherwise the inherent weight leads to permanent deformation, such as bends.

2. Which elastomers are tempered?

Whether rubber or silicone components are tempered depends primarily on the chemical composition of the rubber compound. There are base polymers that need to be tempered more than others. These include all silicone rubbers (LSR and HTV), FKM and HNBR. This does not mean, however, that all the base polymers mentioned must necessarily be tempered. During the production of the compound, different chemicals are added depending on the desired properties of the finished component; these chemicals react chemically during vulcanization and decompose. Some of these substances may only be present in the final product in very limited quantities. To ensure this, tempering is often used to remove all migration-prone components from the component. However, there are also material variants made of silicone, FKM, and HNBR that do not require tempering (temperature-free).

Whether a material is tempered depends on the chemicals contained in the compound to achieve certain performance characteristics that are otherwise (or only with significant additional costs) unattainable.

HTV silicone
HTV stands for high-temperature vulcanizing silicone rubber (high temperature vulcanizing). The raw material is processed as a solid, malleable mixture in a felt or roll form and molded using compression, transfer mold presses, or injection molding. HTV silicones can be vulcanized by peroxide or addition curing. In both cases, tempering can be used, especially when low values for volatile components, a certain residual compressive deformation, or high thermal resistance are required. Often, HTV silicone is also used as an FDA-certified compound in applications in the food or medical technology industries that require high requirements for odor and degassing.

LSR silicone
LSR (liquid silicone rubber) is a liquid, mostly two-component silicone rubber that is predominantly processed using the injection molding method. However, a tempering process may be necessary if particularly low silica content or specific properties are required that can only be achieved by adding certain chemicals. Alternatively, low-volatile, temperature-free LSR types can also be used that can do without any subsequent heat treatment.

Fluoroplastic
In the case of fluoroplastic rubber, abbreviated FKM, tempering is often part of the manufacturing process because during vulcanization, crack products are formed and the DVR without tempering is usually too high for use as a seal. Furthermore, FKM is very gas-tight, which further restricts its diffusion during vulcanization. Biphenyl and peroxy-linked FKM types require different temperature profiles and treatment times. However, there are also some FKM compounds where post-treatment is shorter or completely eliminated.

HNBR
HNBR is a hydrogenated nitrile rubber that is used in high mechanical and thermal loads as well as in contact with oils and fuels. HNBR compounds are often crosslinked by peroxide. A tempering process may be provided if high requirements for heat resistance, residual compressive deformation and long-term property stability exist. In the case of components that emit little gas or particularly demanding sealing applications, tempering may also be part of the process chain. Depending on the degree of hydrogenation and the compound, other crosslinking systems may also be used. Therefore, no necessarily temperature-dependent cycle can be derived from the material designation HNBR.

3. How is the tempering of elastomer components carried out?

For tempering, convection ovens are usually used that have a step control and an exhaust air system. During tempering, the temperature is continuously measured using measuring probes to ensure that all batches are tempered according to the work plan. Depending on the material, one or more temperature levels are maintained in the oven for a certain period of time; for example, in the case of silicone, 4 hours at 170 °C. The steps involved in tempering usually follow the same process:

1. Prepare the components

Before tempering, the components are tested and, if necessary, cleaned of impurities or visible residues. Subsequently, they are placed on tempering plates, grids, or devices. When layering, care is taken to leave sufficient space between the components so that the circulating air reaches all surfaces. Soft, thin-walled or form-weak parts require a suitable support or support to prevent deformation during tempering. Additionally, only one material is tempered per load to eliminate mutual contamination by diffusible materials.

Tempered sheet in production

Figure 1: Temper plate loaded with components in production

2. Heating up

After loading, the oven is brought to the intended temperature. Depending on the material, the heating can be done directly or in several temperature stages. Gradual heating reduces large temperature differences and can prevent deformation or surface damage in sensitive components. Since the air temperature in the oven does not immediately match the temperature in the component, particularly thick-walled molded parts heat up more slowly inside.

3. Tempern

The actual tempering period begins as soon as the thermally most unfavorable area of the batch has reached the intended temperature range. During this phase, the oven maintains the temperature at the desired level. At the same time, the recirculation air ensures uniform heat transfer and removes the materials exiting from the oven chamber.

Temper furnaces in production

Figure 2: Open Temper Furnace in production

5. Cool down and document

After the retention period has expired, the components are cooled and stored until they reach a temperature and humidity level that corresponds to that of the ambient air. Only then are dimensional, hardness, and functional tests, as well as process documentation, performed.

Time-temperature profile during tempering

Time-temperature profile during tempering: Preheating in two stages to 100 °C and 170 °C, holding time at 170 °C, followed by cooling. The component core follows the oven air at a time-delayed rate. Oven air Component core 170 °C 100 °C Room temperature Warming up Hold time Cool down

Figure 3: Time-temperature profile during the tempering process

Any questions about tempering? We are happy to advise you on choosing the right material and manufacturing your rubber or silicone mold part..